MAXIDURA CI-115
EXTREMELY CRACK RESISTANT NICKEL IRON ALLOY ELECTRODE
FOR WELDING CAST IRON
APPLICATION
PROCEDURE
Sufficient amount of the casting skinshould be removed. Depending on the job thickness a U weld or a double U weldshould be made. Use shortest possible arc length. The pass width should not bemore than twice the diameter of the core wire. Deslag every weld bead and peenthe weld metal carefully. Restrike the arc on the weld metal and never on theparent metal.
TECHNICAL DATA
UTS of the joint ( all weld deposit) : 35-45Kgf/mm
Hardness : 150-190 Brinell
Welding process : Shielded metal arc welding (SMAW)
Welding current : AC/ DC (-)
|
|